Diameter | 1,75 ± 0,2 mm |
Printing temperatuer | 175-200 ℃ |
Heated bed temperatuer | 50-80 ℃ |
Tichtheid | 1,25 ± 0,05 g/cm3 |
Heat deflection temperatuer | 50-60 ℃ |
Melt flow rate | 5-7 g/min (190 ℃ 2,16 kg) |
Treksterkte | ≥ 60 Mpa |
Bending sterkte | ≥ 70 Mpa |
Ferlinging by brek | ≥3,0% |
NW | 1,0 kg |
GW | 1,3 kg |
Lingte | ≈ 330 m |