Diameter | 1,75 ± 0,02 mm |
Printing temperatuer | 205-230 ℃ |
Heated Bed Temperatuer | 50-80 ℃ |
Tichtheid | 1,43 ± 0,05 g/cm3 |
Heat Deflection Temperatuer | / |
Melt Flow Rate | 5-8 g/min (190 ℃ 2,16 kg) |
Treksterkte | / |
Bending Strength | / |
Ferlinging by Break | ≥ 600% |
NW | 1,0 kg |
GW | 1,3 kg |
Lingte | ≈ 290m |