Over-Extrusion

MENENE MATSALAR?

Over-extrusion yana nufin cewa firinta yana fitar da filament fiye da yadda ake buƙata.Wannan yana haifar da wuce haddi na filament ya tara a waje na samfurin wanda ke sa bugu a cikin mai ladabi kuma farfajiyar ba ta da santsi.

 

 

DALILAN DA AKE IYAWA

∙ Nozzle Diamita Ba Daidai ba

∙ Filament Diamita Ba Daidai ba

∙ Saitin Extrusion Ba Kyau ba

 

 

HANYOYIN MAGANCE MATSALAR

 

NozzleDiameter Ba Match

Idan an saita slicing azaman bututun da aka saba amfani dashi zuwa diamita na 0.4mm, amma an maye gurbin firinta tare da ƙaramin diamita, to zai haifar da wuce gona da iri.

 

Duba diamita bututun ƙarfe

Bincika saitin diamita na bututun ƙarfe a cikin software slicing da diamita na bututun ƙarfe akan firinta, kuma tabbatar da cewa sun kasance iri ɗaya.

FilashiDiameter Ba Match

Idan diamita na filament ya fi girma fiye da saitin da ke cikin software na yanka, zai kuma haifar da wuce gona da iri.

 

DUBA DIAMETER FILAMENT

Bincika idan saitin diamita na filament a cikin software slicing yayi daidai da filament ɗin da kuke amfani da shi.Kuna iya samun diamita daga kunshin ko ƙayyadaddun filament.

 

AUNA FILAMENT

Diamita na filament yawanci shine 1.75mm.Amma idan filament ɗin ya fi girma diamita, zai haifar da wuce gona da iri.A wannan yanayin, yi amfani da caliper don auna diamita na filament a nesa da maki da yawa, sannan yi amfani da matsakaicin sakamakon auna azaman ƙimar diamita a cikin software slicing.Ana ba da shawarar yin amfani da madaidaicin filaments tare da daidaitaccen diamita.

 

ESaitin xtrusion Ba Kyau ba

Idan an saita mai yawa extrusion kamar magudanar ruwa da ƙimar extrusion a cikin software slicing da yawa, zai haifar da wuce gona da iri.

 

SATA EXTRUSION MULTIPLIER

Idan har yanzu batun yana nan, duba mai haɓakawa mai haɓakawa kamar ƙimar kwarara da rabon extrusion don ganin ko saitin ya yi ƙasa, yawanci tsoho shine 100%.A hankali rage ƙimar, kamar 5% kowane lokaci don ganin ko an inganta matsalar.