Dyamèt | 1.75 ± 0.2mm |
Tanperati enprime | 175-200 ℃ |
Tanperati kabann chofe | 50-80 ℃ |
Dansite | 1.25 ± 0.05 g/cm3 |
Tanperati Devyasyon Chalè | 50-60 ℃ |
Pousantaj koule fonn | 5-7 g/min (190℃ 2.16kg) |
Fòs rupture | ≥ 60 Mpa |
Fòs koube | ≥ 70 Mpa |
Allongement nan Break | ≥3.0% |
NW | 1.0 kg |
GW | 1.3 kg |
Longè | ≈ 330m |