Ububanzi | 1.75 ± 0.2mm |
Izinga Lokushisa Lokuphrinta | 220-250 ℃ |
Izinga Lokushisa Lombhede | 70-100 ℃ |
Ukuminyana | 1.05 ± 0.02 g/cm3 |
I-Heat Deflection Temperature | 70-80℃ |
Melt Flow Rate | 2-4 g/min (190℃ 2.16kg) |
Amandla Okuqina | ≥ 40 Mpa |
Ukugoba Amandla | ≥ 60 Mpa |
Elongation at Break | ≥ 10.0% |
NW | 1.0 kg |
GW | 1.3 kg |
Ubude | ≈ 400m |