Ububanzi | 1.75 ± 0.2mm |
Izinga Lokushisa Lokuphrinta | 175-200 ℃ |
Izinga Lokushisa Lombhede | 50-80℃ |
Ukuminyana | 1.25 ± 0.05 g/cm3 |
I-Heat Deflection Temperature | 50-60 ℃ |
Melt Flow Rate | 5-7 g/min (190℃ 2.16kg) |
Amandla Okuqina | ≥ 60 Mpa |
Ukugoba Amandla | ≥ 70 Mpa |
Elongation at Break | ≥3.0% |
NW | 1.0 kg |
GW | 1.3 kg |
Ubude | ≈ 330m |